Fluor-elbaite, lepidolite and Ta-Nb oxides from a pegmatite of the 3000 Ma Sinceni Pluton, Swaziland: evidence for lithium-cesium-tantalum (LCT) pegmatites in the Mesoarchean
Journal article   Peer reviewed

Fluor-elbaite, lepidolite and Ta-Nb oxides from a pegmatite of the 3000 Ma Sinceni Pluton, Swaziland: evidence for lithium-cesium-tantalum (LCT) pegmatites in the Mesoarchean

Edward S Grew, Ferdinand Bosi, Linus Ros, Per Kristiansson, Mickey E Gunter, Ulf Halenius, Robert B Trumbull and Martin G Yates
European Journal of Mineralogy, Vol.30(2), pp.205-218
2018
url
https://doi.org/10.1127/ejm/2017/0029-2686View